Project Description
Genuine Plastic`s anti-static masterbatch work by lowering the resistivity of a material so that charges are mobile and therefore will not cause static issues such as dust attraction or electrostatic discharge (ESD).But most plastic materials are electrical insulators and have the ability to support high static build up. Anti-static additives are added to plastics to reduce or eliminate a static build up.
Our team of technical experts have years of knowledge and experience in anti-static technologies and applications. Discuss with us your required application, polymer, time frame and regulatory needs and let us recommend the optimum product and addition level for your project.
Specification
Item No. | Additive content | Recommended dosage | Used in | Remark |
---|---|---|---|---|
GP2335PPTR/ GP240 | 40% | 0.6-2.0% | Core layer | Super high additive content, low dosage |
GP2335PPTROB | 40% | 0.6-2.0% | Core layer | Super high additive content, with optical brightener |
GP2635PPTR/ GP241 | 40% | 0.6-2.0% | Core layer | Super high additive content, antistatic mb with slip property |
Item No. | Additive content | Recommended dosage | Used in | Remark |
---|---|---|---|---|
GP2335PPTRCPP/ GP240CPP | 40% | 2.0-4.0% | Core layer & heat sealing layer | Super high additive content, low dosage, for CPP film, reduce the smoke and oil stain on the Die |
GP230PED | 40% | 1.0-4.0% | Core layer & heat sealing layer | Super high additive content, low dosage, for CPP film, reduce the smoke and oil stain on the Die |
Item No. | Additive content | Recommended dosage | Used in | Remark |
---|---|---|---|---|
GP2335PPTRCPP/GP240CPP | 40% | 2.0-4.0% | Core layer & heat sealing layer | Super high additive content, low dosage, for IPP film, reduce the smoke and oil stain on Die |
GP230PED | 40% | 1.0-4.0% | Core layer & heat sealing layer | Super high additive content, low dosage, for IPP film, reduce the smoke and oil stain on Die |